墙柱面采用湿挂、湿贴施工及楼地面铺贴时,为保证工程质量,建议使用市场上质量优质的粘结剂(石英石专用胶)铺贴。
Wall cylinder with wet hanging, wet construction and foor paving, in order to ensure the quality of the project, it is recommended to use the market quality of high quality binder (quartz stone adhesive)paving.
石英石用于楼地面铺贴时,板材之间要预留大约2mm的接缝,以利于水泥砂浆中的水分蒸发、抵消膨胀应力。大面积铺装时,纵横每5m需设8mm的伸缩缝,以防地面及结构之膨胀、收缩导致石材凸起或破裂。
When quartz stone is used for foor paving,about 2mm joints should be reserved between the plates to facitate the evaporation of water in the cement mortar and offset the expansion sress.When a large area of pavement is nstlled, 8mm expansion joints shall be set every 5m horizontaly and horizontaly to prevent the expansion and contraction of the ground and structure from causing the stone protruding or cracking.
石英石应避免滚摔、碰撞造成板材存的暗裂和损伤。室外堆放时,时间不宜过长,冬季施工应采用岩棉被对石英石进行覆盖,石英石铺贴安装前提前2小时搬入室内解融。雨季施工应盖上防水布以防雨淋湿。
Quartz stone should avoid roling, colision caused by the plate surface cracks and damage.Outdoor stacking, the time should not be too long. winter construction should use rock quilt to cover quartz stone,quartz stone paving 2 hours before installation moved into the indoor meltDuring the rainy season, the construction should be covered with tarps to prevent the rain from getting wet
石英石用于楼地面铺贴且采用边找平边铺贴的施工工艺时,需养护48小时以上,2-3天内不能上人及堆放物品,3-5天后方能收缝。
Quartz stone for floor paving and the use of side leveling side paving construction technology, to maintain more than 48 hours,23 days can not be occupied and stacked goods,3-5days to close the seam.